Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 93.0 °C | 199 °F | |
Lord Adhesives 305 General Purpose, Medium Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Flash Point | 93.0 °C | 199 °F | |
Lord Adhesives 309 General Purpose, Non-Sag, Thixotropic Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 322 Hardener; Closed Cup |
Lord Adhesives 320 / 322 Epoxy Adhesive LORD® 320/322 adhesive is a general purpose, two component epoxy adhesive system formulated for primerless adhesion to automotive sheet molded compounds (SMC). This adhesive system also provides .. |
|||
Flash Point | 93.0 °C | 199 °F | |
Lord Adhesives 363 Two-Component, Fast Set, Modified Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | C Curative; Closed Cup |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | D Curative; Closed Cup |
Lord Adhesives 7542 Urethane Adhesive LORD® 7542 adhesive is an equal-mix, two-component urethane adhesive system used to bond FRP, SMC and other plastics with little surface preparation. This adhesive will also bond primed metals. L.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | |
Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment o.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 309-2D Hardener; Closed Cup |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 310A Resin; Closed Cup |
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive Lord® 310 adhesive is a modified, thixotropic, two-part epoxy adhesive which bonds well to many types of prepared metals, prepared rubber, urethane, and plastics. Originally formulated for primer.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 310B Hardener; Closed Cup |
Lord Adhesives Fusor® 310 A/B Epoxy Adhesive Lord® 310 adhesive is a modified, thixotropic, two-part epoxy adhesive which bonds well to many types of prepared metals, prepared rubber, urethane, and plastics. Originally formulated for primer.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 380NS Resin; Closed Cup |
Lord Adhesives Fusor® 380NS / 383NS Epoxy Adhesive LORD Fusor® 380NS/383NS adhesive is a two-part, rapid-cure epoxy adhesive used to bond fiberglass reinforced plastics (FRP), sheet molded compounds (SMC) and metals.All information provided by Lo.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 253 Resin; Closed Cup |
Lord Adhesives Versilok® 253 / 254 Acrylic Adhesive LORD Versilok® 253/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 262 Resin; Closed Cup |
Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 254 Hardener; Closed Cup |
Lord Adhesives Versilok® 262 / 254 Acrylic Adhesive LORD Versilok® 262/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 262B Resin; Closed Cup |
Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive LORD Versilok® 262B/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 254 Hardener; Closed Cup |
Lord Adhesives Versilok® 262B / 254 Acrylic Adhesive LORD Versilok® 262B/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alum.. |
|||
Flash Point | >= 93.0 °C | >= 199 °F | 265 Resin; Closed Cup |
Lord Adhesives Versilok® 265 / 254 Acrylic Adhesive LORD Versilok® 265/254 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare alumi.. |
|||
Flash Point | 92.8 °C | 199 °F | HPC-3 Curative; Seta |
Lord Adhesives HPC-3B Fluoroelastomer Coating LORD HPC-3B and HPC-3C are two-part, room temperature curing fluoroelastomer coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fuel and flu.. |
|||
Flash Point | 93.0 °C | 199 °F | Open cup |
Dow Corning XIAMETER® PMCPMHX-1107 Fluid 30CS Is chemically equivalent to DOW CORNING® MH 1107 FLUID 30 CST. Polymethylhydrogen siloxane fluid, available in 30 cSt viscosity. 1.55-1.60%SiH.Information provided by Dow Corning |
|||
Flash Point | 93.0 °C | 199 °F | Closed Cup |
Dow Corning XIAMETER® PMCPPMX-0246 Cyclohexasiloxane Is chemically equivalent to DOW CORNING® 246 FLUID. This product is a volatile, low viscosity cyclohexasiloxane fluid for use in skincare, suncare, color cosmetics, hair care, and antiperspirant / .. |
|||
Flash Point | 93.0 °C | 199 °F | closed cup |
Dow Corning Z-1223 DIPHENYLDICHLOROSILANE Information provided by Dow Corning |
|||
Flash Point | 92.8 °C | 199 °F | Method A; ASTM D93 |
ExxonMobil Exxsol™ D220/240 Dearomatized Fluid Availability: Africa & Middle East, Europe, Central America and South America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Flash Point | >= 93.0 °C | >= 199 °F | Closed cup |
Dow Corning 203 Fluid 100% active alkylaryl polysiloxane fluid.Information provided by Dow Corning |
|||
Flash Point | >= 93.0 °C | >= 199 °F | Closed cup |
Dow Corning 2502 Cosmetic Fluid A linear polydimethylsiloxane with randomly distributed alkyl chains for use in skincare, woundcare, haircare, suncare, and color cosmetic applications.Information provided by Dow Corning |
|||
Flash Point | 93.0 °C | 199 °F | |
3M 32662 Black Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Flash Point | 93.0 °C | 199 °F | |
BASF Lupragen® DMI 1,2-Dimethyl Imidazole Formula: C5H8N2CAS: 1739-81-0Description: 1,2-Dimethylimidazole is a colorless to yellowish solid with an amine-like odor. Synonyms: DMI, 1,2-Dimethyl-1H-imidazolApplications: It is used as a Cataly.. |
|||
Flash Point | 93.0 °C | 199 °F | |
3M 32660 Heavy Duty Performance Coating - Part A 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Flash Point | 93.0 °C | 199 °F | |
3M 32665 Green Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Flash Point | 93.0 °C | 199 °F | |
3M 32666 Tan Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Flash Point | 93.0 °C | 199 °F | |
3M 32664 Light Gray Heavy Duty Performance Coating - Part B 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |