Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Kolon
Trade Name SPESIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon SPESIN® KP270BL General Purpose PBT Compound Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent waterproofnessApplications: ConnectorsInformation provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.070 %
0.070 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.018 - 0.023 cm/cm
0.018 - 0.023 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
Flexural Modulus 2.452 GPa
355.6 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C
44.4 µin/in-°F
ASTM D696
Melting Point 224 °C
435 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 166 °C
331 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C
138 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.1
3.1
ASTM D150
Dielectric Strength 28.0 kV/mm
711 kV/in
ASTM D149
Arc Resistance 120 sec
120 sec
ASTM D495
Copyright © lookpolymers.com All Rights Reserved