Mechanical Properties Metric English Comments
Flexural Modulus 2.452 GPa
355.6 ksi
ASTM D790
Network Polymers Kepital® F20-52
Description: Natural Acetal Copolymer, Weather Resistance GradeInformation provided by Network Polymers Inc.
Flexural Modulus 2.452 GPa
355.6 ksi
ASTM D790
Kolon SPESIN® KP270BL General Purpose PBT Compound Resin
Excellent waterproofnessApplications: ConnectorsInformation provided by API-Kolon.
Flexural Modulus 2.452 GPa
355.6 ksi
ASTM D790
Tipco Tipwood® 50 EX 50EX
Description: Tipwood® is a Wood-Fiber Reinforced, Heat Stabilized Polypropylene Compound specially developed by Tipco for Automobile Interiors and Appliance Fascia Applications.Features: Environmen..