Kolon KOPA® KN163HI High Impact Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Kolon
Trade Name Kopa®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOPA® KN163HI High Impact Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubrication and abrasion resistance, excellent chemical resistance, wide usage temperature, good impact absorbing characteristicsInformation provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.30 %
0.30 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
DIN 53505; ASTM D785
Tensile Strength, Ultimate 49.0 MPa
7110 psi
DIN 53455; ASTM D638
Elongation at Break 90 %
90 %
DIN 53455; ASTM D638
Flexural Yield Strength 78.5 MPa
11400 psi
DIN 53455; ASTM D790
Flexural Modulus 2.06 GPa
299 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 8.83 J/cm
16.5 ft-lb/in
DIN 53453; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 220 °C
428 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
DIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
DIN 53461; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 20.0 kV/mm
508 kV/in
ASTM D149/DIN 53481
Arc Resistance 120 sec
120 sec
ASTM D495
Users viewing this material also viewed the following: