Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kleerdex Kydex® P26 Acrylic/PVC Extrusion Compound  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kleerdex Kydex® P26 Acrylic/PVC Extrusion Compound  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact profile extrusion compoundApplications: Extruded profiles for recreational equipment, medical equipment, business equipment, profiles for use in the interior of commercial aircraft.Features: P26 is extremely resistant to cracking and abuse. Extruded profiles made with P26 are extremely resistant to harsh chemicals and solvents and to cleaning agents. P26 offers excellent fire retardancy including UL Std 94 V-0 and 5V ratings and FAA flammability compliance.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 189 %
189 %
ASTM D638
Flexural Yield Strength 62.0 MPa
8990 psi
ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 8.00 J/cm

@Thickness 3.17 mm
15.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
V-0, 5V; UL Standard 94
Users viewing this material also viewed the following: