KiON CERASET® POLYUREASILIZANE 20 (PURS 20)

Category Fluid , Polymer , Thermoset
Manufacturer KiON, A Clariant Business
Trade Name CERASET®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KiON CERASET® POLYUREASILIZANE 20 (PURS 20).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionKiON Ceraset Polyureasilazane is a liquid polymer that can easily be converted to a solid pre-ceramic and then be pyrolyzed to either silicon carbide or silicon nitride-containing ceramics.ApplicationsCeramic precursor infiltrant, polymer infiltration/pyrolysis (PIP), and ceramic fibers.Information provided by KiON, A Clariant Business.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Cured Solid
2.40 g/cc
0.0867 lb/in³
Ceramic
Viscosity 50 cP

@Temperature 20.0 °C
50 cP

@Temperature 68.0 °F
Optical Properties Metric English Comments
Refractive Index 1.4896

@Temperature 23.0 °C
1.4896

@Temperature 73.4 °F
Descriptive Properties Value Comments
%Resin 100% solids as liquid
Appearance Clear to pale yellow