Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYMAG® 30S Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYMAG® 40S Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYMAG® 60S Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYMAG® 80S Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYRAL® 15 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYRAL® 200 SM Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYRAL® 22 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYRAL® 32 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec NH 20 Aluminum Hydroxide Used in the production of glass and ceramic productsaluminum fluoride, cryolite and other aluminum saltsfrits and pigmentsmolecular sievescatalystsrefractory productspigments |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYRAL® 30X Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYRAL® 60 VS1 Al(OH)3 The high quality and performance of our surface treated APYRAL® 40VS1 and APYRAL® 60VS1 powders complete the APRYAL® product range for highly specialized applications. Examples include, excellent.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Nabaltec APYRAL® 8 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Density | 2.40 g/cc @Pressure 100 MPa |
0.0867 lb/in³ @Pressure 14500 psi |
Green Density |
Magyar Aluminum ALO-DN-2S Alumina Reactive Alumina |
|||
Density | 2.40 g/cc @Pressure 100 MPa |
0.0867 lb/in³ @Pressure 14500 psi |
Green Density |
Magyar Aluminum ALO-EL-2S Alumina Reactive Alumina |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | Ceramic |
KiON CERASET® POLYSILAZANE 20 (PSZ 20) General DescriptionKiON Ceraset Polysilazane 20 is a liquid polymer that can easily be converted to a solid pre-ceramic and then be pyrolyzed to either silicon carbide or silicon nitride-containing .. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | Ceramic |
KiON CERASET® POLYUREASILIZANE 20 (PURS 20) General DescriptionKiON Ceraset Polyureasilazane is a liquid polymer that can easily be converted to a solid pre-ceramic and then be pyrolyzed to either silicon carbide or silicon nitride-containing.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
GBC Cerasilâ„¢ 223U Ceramic Has a lower CTE, better thermal shock resistance, lower firing temperature, and lower consistent shrinkage than steatite.Applications: ideal for volume production of small pressed insulators often r.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | Apparent |
Gouda Vuurvast AK 53 E Dense Refractory Brick Description: Because of its very high erosion resistance this brick is applied in e.g. recirculation cyclones for CFB coal fired boilers.Remarks: This data represents average values, obtained from s.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Loctite® Output™ 5404 Heat Cure Silicone Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | Cured |
Chesterton ARC I BX1 Impact & Wear Resistant Epoxy Composite Description: An advanced grade epoxy and urethane composite for the repair and protection of all metal surfaces subjected to severe abrasion and impact. It is normally applied at a thickness of 6 mm.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | Cured |
Chesterton ARC MX2 High Wear Fine Particle Wear Compound Description: An advanced ceramic composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion and chemical attack. It is applied at a thickness of 3 mm (1/8”.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Arlon AD255 Woven Glass and PTFE Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Anderman Ceramics EM80P Corundum Porous synthetic mullite with very high thermal shock. Available as tube, sheath, or rod up to 10 ft (3 m) long with diameters 0.3" to 20".Information provided by Anderman Ceramics. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | ISO 1183/A |
Addiplast Addilene H 420 K24 Polypropylene Homopolymer High densityInformation provided by Addiplast. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Arlon AD320 Glass, PTFE and Micro-Dispersed Ceramic Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED). |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
3M W-210 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
3M W-410 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
3M W-610 Ceramic Microspheres 3M™ White Ceramic Microspheres are unique, semi-transparent, white-colored, fine particle size, high-strength microspheres. These products are typically used to reduce VOC levels; increase filler l.. |
|||
Density | 2.40 g/cc | 0.0867 lb/in³ | |
Loctite® 3887 High Adhesion Isotropic Epoxy Adhesive Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditiona.. |