Kennametal Stellite Deloro® 40G

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Deloro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Deloro® 40G.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nickel base. Good combination of wear resistance, corrosion resistance, machinability, and repairability. Machined with tungsten carbide tools, using slow speeds and light feeds. Finish grinding achieved with vitrified silicon carbine wheels. Applications include bottle making mold components such as neck rings, half bushings, and die inserts, also used for sealing faces in values in both the oil and nuclear industries. Normally resistant to atmospheric, steams salt water and salt spray corrosion. Excellent oxidation resistance up to melting range. Satisfactory performance in many organic acids but high corrosion rates observed in hot, strong inorganic acids. Highly resistant to semi-molten glass. Normally used in the as-cast condition. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc.
Physical Properties Metric English Comments
Density 8.20 g/cc
0.296 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 312
312
Converted from Rockwell C hardness.
Hardness, Knoop 372
372
Converted from Rockwell C hardness.
Hardness, Rockwell A 67
67
Converted from Rockwell C hardness.
Hardness, Rockwell B 107
107
Converted from Rockwell C hardness. Beyond normal Rockwell B range, for comparison only.
Hardness, Rockwell C 30 - 38
30 - 38
Hardness, Vickers 326
326
Converted from Rockwell C hardness.
Tensile Strength, Ultimate 385 MPa
55800 psi
Tensile Strength, Yield 350 MPa
50800 psi
Elongation at Break 1.0 %
1.0 %
Modulus of Elasticity 198 GPa
28700 ksi
Charpy Impact, Unnotched 4.00 J

@Temperature 23.0 °C
2.95 ft-lb

@Temperature 73.4 °F
Thermal Properties Metric English Comments
CTE, linear 11.4 µm/m-°C

@Temperature 20.0 - 100 °C
6.33 µin/in-°F

@Temperature 68.0 - 212 °F
12.8 µm/m-°C

@Temperature 20.0 - 300 °C
7.11 µin/in-°F

@Temperature 68.0 - 572 °F
13.4 µm/m-°C

@Temperature 20.0 - 500 °C
7.44 µin/in-°F

@Temperature 68.0 - 932 °F
14.3 µm/m-°C

@Temperature 20.0 - 700 °C
7.94 µin/in-°F

@Temperature 68.0 - 1290 °F
15.4 µm/m-°C

@Temperature 20.0 - 900 °C
8.56 µin/in-°F

@Temperature 68.0 - 1650 °F
Melting Point 985 - 1180 °C
1810 - 2160 °F
Solidus 985 °C
1810 °F
Liquidus 1180 °C
2160 °F
Component Elements Properties Metric English Comments
Boron, B 1.2 %
1.2 %
Carbon, C 0.25 %
0.25 %
Chromium, Cr 7.4 %
7.4 %
Iron, Fe 5.3 %
5.3 %
Nickel, Ni 82 %
82 %
As Remainder
Silicon, Si 4.0 %
4.0 %