Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.33 µin/in-°F @Temperature 68.0 - 212 °F |
|
Kennametal Stellite Deloro® 40G Nickel base. Good combination of wear resistance, corrosion resistance, machinability, and repairability. Machined with tungsten carbide tools, using slow speeds and light feeds. Finish grinding ach.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 21.0 - 399 °C |
6.33 µin/in-°F @Temperature 69.8 - 750 °F |
|
Latrobe HS-105â„¢ ASTM M35 DIN 1.3243 High Speed Steel HS-105 high speed steel is a cobalt-modified M2 high speed steel in which the cobalt addition provides hot hardness that is intermediate between those of M2 and M42 high speed steels. The improved h.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 1000 °C |
6.33 µin/in-°F @Temperature 1830 °F |
|
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 315 °C |
6.33 µin/in-°F @Temperature 68.0 - 599 °F |
|
Latrobe 440â„¢ N-DUR High Quality Martensitic Stainless Steel 440 N-DUR is a 15.0% chromium stainless steel that provides the corrosion resistance of 440 C with the added benefit of improved carbide size and distribution for noiseless miniature precision beari.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 600 °C |
6.33 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Corning Macor® Machinable Glass Ceramic The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 400 °C |
6.33 µin/in-°F @Temperature 68.0 - 752 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 600 °C |
6.33 µin/in-°F @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 600 °C |
6.33 µin/in-°F @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER S590 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature <=538 °C |
6.33 µin/in-°F @Temperature <=1000 °F |
|
AK Steel 430 Ferritic Stainless steel AK Steel 430 combines good corrosion resistance and heat and oxidation resistance up to 1500°F with good mechanical properties. Typical consumer applications include automotive trim and molding, f.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature <=538 °C |
6.33 µin/in-°F @Temperature <=1000 °F |
|
AK Steel 434 Ferritic Stainless steel AK Steel 434 is a modification of Type 430, the addition of molybdenum increases this alloy's corrosion resistance and its attack from many deicing chemicals. It also provides good heat and oxidati.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 400 °C |
6.33 µin/in-°F @Temperature 68.0 - 752 °F |
|
Assab Steels DF-3 Cold Work Steel DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 538 °C |
6.33 µin/in-°F @Temperature 68.0 - 1000 °F |
|
ATI Allegheny Ludlum AL 453™ Stainless Steel Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 600 °C |
6.33 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 37.8 - 427 °C |
6.35 µin/in-°F @Temperature 100 - 800 °F |
|
Crucible Steel REX® M7N High Speed Steel, AISI M7 REX M7 is molybdenum type high speed steel designed with higher carbon and vanadium to provide higher hardness after heat treatment and improved wear resistance compared to M1 steel.Information prov.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.33 µin/in-°F @Temperature 68.0 - 212 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |