Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.33 µin/in-°F @Temperature 68.0 - 212 °F |
|
Kennametal Stellite Deloro® 40G Nickel base. Good combination of wear resistance, corrosion resistance, machinability, and repairability. Machined with tungsten carbide tools, using slow speeds and light feeds. Finish grinding ach.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 21.0 - 399 °C |
6.33 µin/in-°F @Temperature 69.8 - 750 °F |
|
Latrobe HS-105â„¢ ASTM M35 DIN 1.3243 High Speed Steel HS-105 high speed steel is a cobalt-modified M2 high speed steel in which the cobalt addition provides hot hardness that is intermediate between those of M2 and M42 high speed steels. The improved h.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 1000 °C |
6.33 µin/in-°F @Temperature 1830 °F |
|
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, 6.3 mm plate The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 315 °C |
6.33 µin/in-°F @Temperature 68.0 - 599 °F |
|
Latrobe 440â„¢ N-DUR High Quality Martensitic Stainless Steel 440 N-DUR is a 15.0% chromium stainless steel that provides the corrosion resistance of 440 C with the added benefit of improved carbide size and distribution for noiseless miniature precision beari.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 600 °C |
6.33 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Corning Macor® Machinable Glass Ceramic The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 400 °C |
6.33 µin/in-°F @Temperature 68.0 - 752 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 600 °C |
6.33 µin/in-°F @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 600 °C |
6.33 µin/in-°F @Temperature 1110 °F |
|
Bohler-Uddeholm BÖHLER S590 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature <=538 °C |
6.33 µin/in-°F @Temperature <=1000 °F |
|
AK Steel 430 Ferritic Stainless steel AK Steel 430 combines good corrosion resistance and heat and oxidation resistance up to 1500°F with good mechanical properties. Typical consumer applications include automotive trim and molding, f.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature <=538 °C |
6.33 µin/in-°F @Temperature <=1000 °F |
|
AK Steel 434 Ferritic Stainless steel AK Steel 434 is a modification of Type 430, the addition of molybdenum increases this alloy's corrosion resistance and its attack from many deicing chemicals. It also provides good heat and oxidati.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 400 °C |
6.33 µin/in-°F @Temperature 68.0 - 752 °F |
|
Assab Steels DF-3 Cold Work Steel DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 538 °C |
6.33 µin/in-°F @Temperature 68.0 - 1000 °F |
|
ATI Allegheny Ludlum AL 453™ Stainless Steel Single phase iron-chromium ferritic stainless steel alloy. Should be annealed between 1450 and 1600°F and quickly cooled. Information provided by Allegheny Ludlum |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 600 °C |
6.33 µin/in-°F @Temperature 77.0 - 1110 °F |
|
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 25.0 - 300 °C |
6.33 µin/in-°F @Temperature 77.0 - 572 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |
|||
CTE, linear | 11.4 µm/m-°C @Temperature 20.0 - 100 °C |
6.33 µin/in-°F @Temperature 68.0 - 212 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |