Mechanical Properties Metric English Comments
Tensile Strength, Yield 350 - 460 MPa

@Strain 0.200 %
50800 - 66700 psi

@Strain 0.200 %
after heat treatment
PEAK Werkstoff DISPAL S691 Aluminum Alloy, AlCu5Ti
High stiffness and elongation at ruptureInformation provided by PEAK Werkstoff GmbH
Tensile Strength, Yield 350 MPa
50800 psi
Kennametal Stellite Deloro® 40G
Nickel base. Good combination of wear resistance, corrosion resistance, machinability, and repairability. Machined with tungsten carbide tools, using slow speeds and light feeds. Finish grinding ach..
Tensile Strength, Yield 350 MPa
50800 psi
Proof Stress
Kennametal Stellite Denertiaâ„¢ N8 Nickel Dental Alloy
Denertiaâ„¢ N8 is a low-carbon nickel based porcelain-bonding alloy for the manufacture of dental crowns and bridges.This alloy is Beryllium and Cadmium free as defined by ISO 22674Information pr..
Tensile Strength, Yield 350 MPa
50800 psi
MMCC Aluminum/SiC 55p Aluminum Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Tensile Strength, Yield >= 350 MPa
>= 50800 psi
MetalTek MTEK 50-50Nb Cast UNS R20501 Heat Resistant Stainless Steel
Information provided by MetalTek
Tensile Strength, Yield 350 MPa

@Strain 0.200 %
50800 psi

@Strain 0.200 %
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Tensile Strength, Yield 350 MPa

@Strain 0.200 %
50800 psi

@Strain 0.200 %
Haynes 230® alloy, plate, 8000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applic..
Tensile Strength, Yield 350 MPa

@Strain 0.200 %
50800 psi

@Strain 0.200 %
Haynes 625 alloy, 50% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
Tensile Strength, Yield 350 MPa

@Temperature 870 °C
50800 psi

@Temperature 1600 °F
Haynes Hastelloy® alloy 188 12.7 mm plate weldments
Solid solution-strengthened developed as a filler metal for welding of dissimilar alloys. Applications include excellent dissimilar welding characteristics in the gas turbine, aerospace, and chemica..
Tensile Strength, Yield 350 MPa

@Strain 0.200 %,
Temperature 650 °C
50800 psi

@Strain 0.200 %,
Temperature 1200 °F
Special Metals UDIMET® alloy 188 Cobalt-base Alloy
UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small ..
Tensile Strength, Yield 350 - 420 MPa

@Strain 0.200 %
50800 - 60900 psi

@Strain 0.200 %
SSAB Tunnplat Aluzink 350A YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Aluzink YP - HSLA steel (aluminum-zinc coated sheet). Property values are for thicknesses 0.4 - 2.0 mm. Iron content is approximate - exact composition is ..
Tensile Strength, Yield 350 - 440 MPa

@Strain 0.200 %
50800 - 63800 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 350YP High-strength Steel
High-strength SteelComments: Docol YP - Cold Rolled Steel - HSLA. Property values are for cold-rolled steel; thicknesses 0.5 - 3.00 mm. Iron content is approximate - exact composition is not report..
Tensile Strength, Yield 350 - 440 MPa

@Strain 0.200 %
50800 - 63800 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 600DP High-strength Steel
High-strength SteelComments: Docol DP - Cold Rolled Steel - Extra high-strength steel (EHS). Property values are for cold-rolled steel; thicknesses 0.5 - 1.6 mm. Iron content is approximate - exact..
Tensile Strength, Yield 350 - 420 MPa

@Strain 0.200 %
50800 - 60900 psi

@Strain 0.200 %
SSAB Tunnplat Dogal 350YP High-strength Metal-coated Steel
High-strength Metal-coated SteelComments: Dogal YP - HSLA steel. Property values are for thicknesses 0.4 to 2.5 mm. Iron content is approximate - exact composition is not reported by the manufactur..
Tensile Strength, Yield 350 MPa
50800 psi
SSAB Tunnplat Domex® 024 BOR Rolled Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield >= 350 MPa
>= 50800 psi
SSAB Tunnplat Domex® 350XP Extra High-strength Cold-forming Steel
Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene..
Tensile Strength, Yield >= 350 MPa
>= 50800 psi
SSAB Tunnplat Domex® 350YP Cold-forming Steel, HSLA
Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex®..
Tensile Strength, Yield >= 350 MPa

@Strain 0.200 %
>= 50800 psi

@Strain 0.200 %
CLAL-MSX NICLAL 1300 H12 1/2 Hard Copper Alloy, Free Cutting Nickel-Silver
Main Characteristics: Good ductilityGood corrosion resistanceTypical Applications:High volume turned partsKeysInformation provided by CLAL-MSX
Tensile Strength, Yield 350 MPa

@Temperature 700 °C
50800 psi

@Temperature 1290 °F
R<sub>p</sub>02
Assab Steels QRO 90 SUPREME Hot Work Steel
QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista..
Tensile Strength, Yield 350 - 550 MPa
50800 - 79800 psi
before hot stamping
ArcelorMittal Usibor® 1500 Ultra high strength steel, Cold Rolled
Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to ..
Tensile Strength, Yield 350 - 550 MPa
50800 - 79800 psi
before hot stamping
ArcelorMittal Usibor® 1500 Ultra high strength steel, Hot Rolled
Description: Usibor® 1500 and 22MnB5 are hot formed grades intended for use in automobile structural and safety components. The very high mechanical strength of the final part makes it possible to ..
Tensile Strength, Yield 350 MPa
50800 psi
AK Steel DI-MAX® HF-10 Nonoriented Electrical Steel
DI-MAX HF-10 is a fully processed nonoriented electrical steel designed for use in high speed motors, traction motors, aircraft generators, and other rotating equipment operating at frequencies abov..
Tensile Strength, Yield 350 MPa

@Strain 0.200 %
50800 psi

@Strain 0.200 %
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications ..
Tensile Strength, Yield 350 MPa

@Strain 0.200 %
50800 psi

@Strain 0.200 %
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications ..
Tensile Strength, Yield 350 MPa

@Strain 0.200 %
50800 psi

@Strain 0.200 %
Haynes 230® alloy, plate, 4000 hours exposure at 871°C (1600°F)
Excellent high-temperature strength, outstanding resistance to oxidizing environments up to 1149°C, premier resistance to nitriding environments, and excellent long-term thermal stability. Applicat..