Karina 651D28/29-D-IS ICE PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Karina 651D28/29-D-IS ICE PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fungi resistant PVC compound, recommended for injection of bathroom carpet.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D 792
ASTM Color -1.89 - 1.11
-1.89 - 1.11
Color A, ME 12
-1.46 - 1.54
-1.46 - 1.54
Color B, ME 12
60.54 - 63.54
60.54 - 63.54
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 63 - 67

@Time 15.0 sec
63 - 67

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 9.81 MPa
>= 1420 psi
ASTM D 638
Elongation at Break >= 300 %
>= 300 %
ASTM D 638