Material Notes:
Filled with mineralsInformation provided by Qualchem Zrt.
Physical Properties Metric English Comments
Filler Content 8.0 - 12 %
8.0 - 12 %
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
50 mm/min; ISO 527-1,2
Elongation at Break 3.0 %
3.0 %
ISO 527-1,2
Charpy Impact Unnotched 4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 4.00 mm
HB

@Thickness 0.157 in
MSZ 10383
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
DIN 53482
Comparative Tracking Index 450 V
450 V
IEC 112
Processing Properties Metric English Comments
Moisture Content 2.0 - 2.2 %
2.0 - 2.2 %
DIN 53714