Material Notes:
Highest brightness, smallest particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, Butyl Rubber, General Plastics, Polyolefins/PVC, Thermoset, Thermoplastic, EPDM, Masterbatch, Wire & CableInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.63 g/cc
2.63 g/cc
Bulk Density 0.224 - 0.400 g/cc
0.00810 - 0.0145 lb/in³
Loose
Solids Content 50 - 51 %
50 - 51 %
Slurry
Brightness 92 - 93.5 %
92 - 93.5 %
Reflectance (TAPPI)
Oil Absorption 65 %
65 %
Fineness >= 5
>= 5
Hegman Grind
Moisture Absorption at Equilibrium <= 0.5 %
<= 0.5 %
As Produced
Particle Size 0.600 µm
0.600 µm
Average Stokes Equivalent Diameter
1.50 µm
1.50 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6 - 8
6 - 8
100 g/250 ml H2O Slurry
Specific Surface Area 16.0 m²/g
16.0 m²/g
BET
Descriptive Properties Value Comments
Bulking Value 21.9 lb.gal
CAS Number 92704-41-1
Crystalline Silica (quartz) <0.1%
Physical Forms Dry, Slurry