Physical Properties Metric English Comments
Bulk Density 0.300 - 0.400 g/cc
0.0108 - 0.0145 lb/in³
Oceanchem Group Melamine Cyanurate (MCA)
Molecular Formula: C6H9N9O3Cas No.: 37640-57-6Physical Appearance: Fine, white, crystalline powder, nontoxic, odorless; indissolvable in water and most organic solvents.Use: Melamine Cyanurate is a ..
Bulk Density 0.250 - 0.400 g/cc
0.00903 - 0.0145 lb/in³
Magyar Aluminum ALOLT 120F Aluminum Hydroxide
Fine Precipitated Type
Bulk Density 0.280 - 0.400 g/cc
0.0101 - 0.0145 lb/in³
ASTM D1895
LG Chemical LP170 PVC
General Description: LP170, homopolymer made from micro- suspension polymerization, is a medium- viscosity PVC resin with a pseudo plastic flow property in processing range. LP170 can be used for sy..
Bulk Density 0.300 - 0.400 g/cc
0.0108 - 0.0145 lb/in³
ASTM D1895
LG Chemical PA1302 PVC
General Description: PA1302, vinyl chloride copolymer with vinyl acetate exhibits excellent properties. It is easy to process and gives effective flow. Main Applications: Adhesive for sheet & film, ..
Bulk Density 0.300 - 0.400 g/cc
0.0108 - 0.0145 lb/in³
ASTM D1895
LG Chemical PB1752 PVC
General Description: PB1752, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for sk..
Bulk Density 0.300 - 0.400 g/cc
0.0108 - 0.0145 lb/in³
ASTM D1895
LG Chemical PB900 PVC
General Description: PB900, homopolymer made by micro-suspension seeded polymerization, is PVC resin with pseudo plastic flow property. PB900 can be used for wall paper made by knife coating/rotary ..
Bulk Density 0.224 - 0.400 g/cc
0.00810 - 0.0145 lb/in³
Loose
KaMin KaMin® 2000C Kaolin Clay - Calcined
Highest brightness, smallest particle size, calcined kaolin clay, more cost -effective Ti02 extender than KaMin® 70C.Industry: Paint & CoatingsUses: Architectural Coatings, Industrial Coatings, F..
Bulk Density 0.224 - 0.400 g/cc
0.00810 - 0.0145 lb/in³
Loose
KaMin Polyfil® 90 Kaolin Clay - Calcined
Highest brightness, smallest particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, Butyl Rubber, General Plastics, Polyolefins/PVC, Thermoset, Thermo..
Bulk Density 0.200 - 0.400 g/cc
0.00723 - 0.0145 lb/in³
HG/T 2900
Shanghai Ofluorine T-2 PVDF for Powder Coatings
Description: T-2 PVDF belong to thermoplastic fluorocarbon resin, which has high melt flow rate, low melt viscosity. T-2 PVDF has characteristic of chemical resistance, heat resistance, high mechani..
Bulk Density 0.200 - 0.400 g/cc
0.00723 - 0.0145 lb/in³
Dow Corning EP-9289 LL Cosmetic Powder
A white cross-linked dimethyl polysiloxane elastomer powder combined with lauroyl lysine. This unique combination enables the powder to improve flow and reduce agglomeration, providing superior hand..