Physical Properties Metric English Comments
Particle Size 1.50 µm
1.50 µm
Median (Malvern Laser)
KaMin KaMin® 2000C Kaolin Clay - Calcined
Highest brightness, smallest particle size, calcined kaolin clay, more cost -effective Ti02 extender than KaMin® 70C.Industry: Paint & CoatingsUses: Architectural Coatings, Industrial Coatings, F..
Particle Size 1.50 µm
1.50 µm
Median (Malvern Laser)
KaMin KaMin® 90 Kaolin clay - Waterwashed
KaMin® 90 is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90 is ideally suited for solvent and water-borne paint, ink and adhesive applicati..
Particle Size 1.50 µm
1.50 µm
Median (Malvern Laser)
KaMin KaMin® 90B Kaolin Clay - Waterwashed
KaMin® 90B is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90B is ideally suited for water-borne applications where high gloss, holdout and ..
Particle Size 1.50 µm
1.50 µm
Median (Malvern Laser)
KaMin Polyfil® 90 Kaolin Clay - Calcined
Highest brightness, smallest particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, Butyl Rubber, General Plastics, Polyolefins/PVC, Thermoset, Thermo..
Particle Size 1.50 µm
1.50 µm
Median (Malvern Laser)
KaMin Polyfil® F Kaolin Clay - Waterwashed
Water washed kaolin clays such as Polyfil® F offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® F is a moderate brightness water ..
Particle Size 1.50 µm
1.50 µm
Median (Malvern Laser)
KaMin Polyfil® FB Kaolin Clay - Waterwashed
Water washed kaolin clays such as Polyfil® FB offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® FB is a moderate brightness wate..
Particle Size 1.50 µm
1.50 µm
Median (Malvern Laser)
KaMin Polyfil® WC-426 Kaolin Clay - Calcined
Fine particle size vinyl-functional calcined clay for outstanding wet electricals and long term stability in wire and cable applications.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rub..
Particle Size 1.50 - 2.50 µm
1.50 - 2.50 µm
Average value: 1.83 µm Grade Count:3
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is ..
Particle Size 1.50 - 2.50 µm
1.50 - 2.50 µm
Average value: 1.83 µm Grade Count:3
Overview of materials for Linear Low Density Polyethylene (LLDPE), Sheeting Grade