Polymer Property : Specific Surface Area = 16.0 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 16.0 m²/g
16.0 m²/g
BET
KaMin KaMin® 2000C Kaolin Clay - Calcined
Highest brightness, smallest particle size, calcined kaolin clay, more cost -effective Ti02 extender than KaMin® 70C.Industry: Paint & CoatingsUses: Architectural Coatings, Industrial Coatings, F..
Specific Surface Area 16.0 m²/g
16.0 m²/g
BET
KaMin KaMin® 80 Kaolin Clay - Waterwashed
KaMin® 80 is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appli..
Specific Surface Area 16.0 m²/g
16.0 m²/g
BET
KaMin Polyfil® X Kaolin Clay - Waterwashed
Cost effective, kaolin extender offering improved consistency vs air floated clays, pulverized powder form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, SMC/BMC, EPDM, Mold..
Specific Surface Area 16.0 m²/g
16.0 m²/g
BET
KaMin Polyfil® 90 Kaolin Clay - Calcined
Highest brightness, smallest particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, Butyl Rubber, General Plastics, Polyolefins/PVC, Thermoset, Thermo..