Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer Total Atofina
Trade Name HDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFood packagingCoextrusionExtrusion coatingInformation provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM D792
Water Vapor Transmission 3.41 g/m²/day

@Temperature 37.8 °C
0.220 g/100 in²/day

@Temperature 100 °F
ASTM E96/66
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.5 MPa
5000 psi
film; ASTM D882
Elongation at Break 1000 %
1000 %
ASTM D882
Secant Modulus 0.655 GPa
95.0 ksi
ASTM D882
Elmendorf Tear Strength MD 35 g
35 g
ASTM D1922
Elmendorf Tear Strength TD 50 g
50 g
ASTM D1922
Dart Drop Test 85.0 g
0.187 lb
ASTM D1709
Thermal Properties Metric English Comments
Melting Point 129 °C
265 °F
ASTM D3417
Optical Properties Metric English Comments
Haze 15 %
15 %
ASTM D1003
Gloss 65 %
65 %
ASTM D523
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 232 - 260 °C
450 - 500 °F
Extrusion