Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of general purpose, UV stable and low-temperature impact grades for use in a wide range of demanding applications and severe operating environments plus customized formulations to meet specialized requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 54.5 MPa
7900 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 1.65 GPa
239 ksi
ASTM D638
Flexural Strength 80.9 MPa
11700 psi
13 mm/min; ASTM D790
Flexural Modulus 2.12 GPa
307 ksi
13 mm/min; ASTM D790
Izod Impact, Notched 5.70 J/cm

@Thickness 3.18 mm,
Temperature -30.0 °C
10.7 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
Injection Molded; ASTM D256A
7.40 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
13.9 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C

@Thickness 6.35 mm
181 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Features Good Impact Resistance
Good UV Resistance
Good Weather Resistance
Forms Pellets
Generic Material PC+PBT
Generic Name Polycarbonate + PBT (PC+PBT)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America