KYDEX® 6200 Thermoplastic Sheet

Category Polymer , Thermoplastic
Manufacturer KYDEX LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® 6200 Thermoplastic Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fire rated sheet for mass transitApplications: Dashboards, seatbacks, armrests, tray tables, window reveals, cabin linersFeatures: Kydex 6200 is a proprietary, high performance thermoplastic sheet. It is designed for use in mass transit vehicles. It meets the recommended fire safety practices of both the FTA and FRA for smoke emission and flammability as tested. It is the ideal thermoplastic to solve mass transportation equipment needs. Passes Motor Vehicle Safety Standards (MVSS 302).Fabrication: Kydex 6200 forms to deep draws with low forces when heated to the upper range of 176-199°C, and has unusually high resistance to hot tearing. It can be formed on all standard presses, and cut on all standard die-cutting machines.Data provided by the Kleerdex Company.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 55 %
55 %
Modulus of Elasticity 2.413 GPa
350.0 ksi
Flexural Yield Strength 63.0 MPa
9140 psi
ASTM D790
Izod Impact, Notched 1.87 J/cm

@Temperature 23.0 °C
3.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 176 - 199 °C
349 - 390 °F
Draws deep with low force in this range.