Polymer Property : Processing Temperature = 390 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 176 - 199 °C
349 - 390 °F
Draws deep with low force in this range.
KYDEX® 6200 Thermoplastic Sheet
Fire rated sheet for mass transitApplications: Dashboards, seatbacks, armrests, tray tables, window reveals, cabin linersFeatures: Kydex 6200 is a proprietary, high performance thermoplastic sheet. ..