Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Isoflon PVC Polyvinyl Chloride

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Uncompounded
Manufacturer Isoflon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon PVC Polyvinyl Chloride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good mechanical propertiesThermoformableGood impact resistanceInformation provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
DIN 53479
Water Absorption 0.20 %
0.20 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
ASTM D785
Elongation at Break 45 - 54 %
45 - 54 %
DIN 53455
Tensile Modulus 2.50 GPa
363 ksi
DIN 53457
Thermal Properties Metric English Comments
CTE, linear 70.0 - 80.0 µm/m-°C
38.9 - 44.4 µin/in-°F
DIN 52328
Thermal Conductivity 0.120 W/m-K
0.833 BTU-in/hr-ft²-°F
DIN 52612
Melting Point 160 °C
320 °F
DIN 53736
Maximum Service Temperature, Air 60.0 °C
140 °F
Continuous; DIN 52612
Minimum Service Temperature, Air 0.000 °C
32.0 °F
Continuous; DIN 52612
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
DIN 53482
Dielectric Constant 3.3

@Frequency 1000 Hz
3.3

@Frequency 1000 Hz
DIN 53483
Dielectric Strength 35.0 - 50.0 kV/mm
889 - 1270 kV/in
DIN 53481
Descriptive Properties Value Comments
Color Gray/ivory
Fire Rating M1-M2
CSTB
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved