Material Notes:
The grade is a medium flow heterophasic the copolymer mainly designed for injection molding application.Application: containers, buckets, pails, crates and also used for automotive parts.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 3.5 g/10 min
3.5 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ISO 868
Tensile Stress 26.0 MPa
3770 psi
ISO R527
Elongation at Yield 10 %
10 %
ISO R527
Flexural Modulus 1.15 GPa
167 ksi
ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 151 °C
304 °F
ISO 306/A
Heat Distortion Temperature 88.0 °C
190 °F
ISO 75/B