Polymer Property : Tensile Stress = 26.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 26.0 MPa
3770 psi
ISO R527
Iran Petrochemical (PCC) EP-C 30 R Polypropylene
The grade is a heterophasic polypropylene copolymer for injection molding the product offers an excellent balance of stiffness.Application: automotive parts, wells, garden furniture, chair shells an..
Tensile Stress 26.0 MPa
3770 psi
ISO R527
Iran Petrochemical (PCC) EPD 60 R Polypropylene
EPD 60 R has a high molecular weight giving it superior toughness even at low temperature. It has excellent heat and detergent resistance.Applications: extrusion blow molding applications include t..
Tensile Stress 26.0 MPa
3770 psi
ISO R527
Iran Petrochemical (PCC) EP-T 30 R Polypropylene
The grade is a medium flow heterophasic the copolymer mainly designed for injection molding application.Application: containers, buckets, pails, crates and also used for automotive parts.Informatio..
Tensile Stress 26.0 MPa

@Strain 1.00 %,
Time 3.60e+6 sec
3770 psi

@Strain 1.00 %,
Time 1000 hour
DIN 53444
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified
Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex