Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 151 °C | 304 °F | Rate A; 4 mm thick;10.0 mm wide molded rod; ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 923ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 943 PC Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 943ASR PC (Asia Pacific) More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 940A PC Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 950A PC (Asia Pacific) Transparent, clear and colors, high viscosity, flame retardant with exceptional surface. |
|||
Vicat Softening Point | 151 °C @Load 5.10 kg |
304 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1200-03 Polycarbonate Resin Description: LUPOY PC 1200-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 151 °C @Load 5.10 kg |
304 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1201-05 Polycarbonate Resin Description: LUPOY PC 1201-05 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 151 °C | 304 °F | ISO 306/A |
Iran Petrochemical (PCC) EP-C 30 R Polypropylene The grade is a heterophasic polypropylene copolymer for injection molding the product offers an excellent balance of stiffness.Application: automotive parts, wells, garden furniture, chair shells an.. |
|||
Vicat Softening Point | 151 °C @Load 5.10 kg |
304 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1300-03 Polycarbonate Resin Description: LUPOY PC 1300-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 151 °C @Load 5.10 kg |
304 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1302HP-09 Polycarbonate Resin Description: LUPOY PC 1302HP-09 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
Vicat Softening Point | 151 °C | 304 °F | ASTM D1525 |
Ineos N01G-02 Polypropylene Impact Copolymer N01G-02 is a low melt flow rate polypropylene impact copolymer designed for blow molding, extrusion, and compounding applications. The grade benefits from a very high impact resistance at room and l.. |
|||
Vicat Softening Point | 151 °C | 304 °F | ISO 306/A |
Iran Petrochemical (PCC) EPV 31 RA Polypropylene A high fluidity heterophasic copolymer for thin wall injection molding exhibits high stiffness, relatively good impact residence.Applications: flower pots, containers, filters, house wares.Informati.. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate A/120; ISO 306 |
SABIC Innovative Plastics NORYL PX9406P PPE+HIPS (Asia Pacific) Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 125dc HDT. UL94 V-0 rated. Electrical applications. |
|||
Vicat Softening Point | 151 °C | 304 °F | 50°C/hr, 50N Load; ASTM D1525 |
Styron CALIBREâ„¢ 201-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 151 °C @Load 5.10 kg |
304 °F @Load 11.2 lb |
Rate A (50°C/h); ASTM D1525 |
Styron CALIBREâ„¢ 201-6 Polycarbonate Resin Overview: CALIBREâ„¢ 201-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance.. |
|||
Vicat Softening Point | 151 °C | 304 °F | 50°C/hr, 50N; ASTM D1525 |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Vicat Softening Point | 151 °C | 304 °F | 50°C/hr, 50N Load; ASTM D1525 |
Styron CALIBREâ„¢ 303-06 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 151 °C | 304 °F | 50°C/hr, 50N; ASTM D1525 |
Styron CALIBREâ„¢ 893-20 Polycarbonate CALIBREâ„¢ 893-20 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo.. |
|||
Vicat Softening Point | 151 °C | 304 °F | ISO 306 |
Unipetrol PP MONSTEN® MA 745 Polypropylene Impact Copolymer Made for injection molding applications. Antistatic stabilization. Impact copolymer.Information provided by Unipetrol RPA |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate A; ASTM D1525 |
Covestro Makrolon® 6255 Polycarbonate, Flame Retardant, High Productivity, Mold Release Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Vicat Softening Point | 151 °C | 304 °F | A50 (10N); ISO 306 |
Domo 2300L Polypropylene Copolymer Information provided by Domo. |
|||
Vicat Softening Point | 151 °C | 304 °F | 10 N; ASTM D1525 |
Braskem H 504 XP Bioriented Film Polypropylene Description: H 504XP is a low melt flow rate homopolymer, designed specially for high speed lines of biorented films (BOPP). This product features a broad processing window with high output and regu.. |
|||
Vicat Softening Point | 151 °C | 304 °F | ISO 306/A50 |
Addiplast Addilene J 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Vicat Softening Point | 151 °C | 304 °F | ISO 306/A50 |
Addiplast Addilene J 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Vicat Softening Point | 151 °C | 304 °F | ISO 306/A50 |
Addiplast Addilene J 510 Polypropylene Copolymer UnreinforcedInformation provided by Addiplast. |
|||
Vicat Softening Point | 151 °C | 304 °F | A (10N); ISO 306 |
Borealis Xmod™ MC55T1 Polypropylene Compound 10% Mineral Filled Xmod MC55t1 is a 10% mineral filled grade based on HCPP intended for injection molding. Xmod has been developed especially for the car industry, to be used in interior parts. XMod offers very good .. |
|||
Vicat Softening Point | 151 °C | 304 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 940 PC Opaque colors, medium viscosity, superior flame retardance. |