Intercontinental Polymers 555 PBT Polymer Elastomer Polyester Pellets

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer Intercontinental Polymers, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Intercontinental Polymers 555 PBT Polymer Elastomer Polyester Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Engineering Resin - ModifiedInformation provided by Intercontinental Polymers.
Physical Properties Metric English Comments
Relative Viscosity 1.985 - 2.135 cP
1.985 - 2.135 cP
LCL-PR21
Melt Flow 37 g/10 min
37 g/10 min
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
Optical Properties Metric English Comments
Gardner Color Number 7.5 - 11.5
7.5 - 11.5
+ b; LCL-PR01
77 - 89
77 - 89
Rd; LCL-PR01
Processing Properties Metric English Comments
Melt Temperature 174 °C
345 °F
LCL-PR29
Descriptive Properties Value Comments
Black Specks Max. 10/200 g
LCL-PR05