Relative Viscosity 1.985 - 2.135 cP
1.985 - 2.135 cP
LCL-PR21
Intercontinental Polymers 555 PBT Polymer Elastomer Polyester Pellets
Applications: Engineering Resin - ModifiedInformation provided by Intercontinental Polymers.