Material Notes:
This is a polypropylene homopolymer for general purpose injection molding and high speed spinning applications. It is useful for spun bonded nonwovens and partially oriented yarn (POY). This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsFiber and tapeGeneral purpose injection moldingNonwoven fabricsPartially oriented yarnStaple fiberBenefitsExcellent gas fade resistanceExcellent processabilityHigh line speedsNarrow molecular weight distributionInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 38 g/10 min

@Load 2.16 kg,
Temperature 230 °C
38 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.75 MPa

@Temperature 23.0 °C
5475 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Elongation at Yield 8.9 %
8.9 %
ASTM D638
Flexural Modulus 1.58 GPa

@Temperature 23.0 °C
229 ksi

@Temperature 73.4 °F
ASTM D790A
Izod Impact, Notched 0.267 J/cm

@Temperature 23.0 °C
0.500 ft-lb/in

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
227 °F
ASTM D648
Descriptive Properties Value Comments
Process Fiber
Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: