Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 37.75 MPa @Temperature 23.0 °C |
5475 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos H38G-02 Polypropylene Homopolymer This is a polypropylene homopolymer for general purpose injection molding and high speed spinning applications. It is useful for spun bonded nonwovens and partially oriented yarn (POY). This mater.. |