Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 227 °F | ASTM D648 |
Ineos H38G-02 Polypropylene Homopolymer This is a polypropylene homopolymer for general purpose injection molding and high speed spinning applications. It is useful for spun bonded nonwovens and partially oriented yarn (POY). This mater.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 227 °F | ASTM D648 |
Plastics Group Polifil® RMC-30 30% Calcium Carbonate-Reinforced Polypropylene, High Impact Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 227 °F | ASTM D648 |
Westlake Plastics Propylux® SD-A Polypropylene (anti-static) Non-carbon-filled, permanently static-dissipative material, with good chemical resistance and mechanical properties. This material is light weight, weldable, easily machined and fabricated, availab.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 108 °C | 227 °F | ASTM D648 |
ExxonMobil AXO3BE3 Polypropylene Homopolymer Product Description: A high crystallinity, medium impact copolymer resin designed for injection-molded automotive interior applications and large appliance parts applications requiring high melt fl.. |