Ineos A4040 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos A4040 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ineos HDPE A4040 is a high density polyethylene copolymer produced using a supported catalyst process. It is a copolymer resin used mainly for the extrusion of crosslinked pipes according to the silane process.
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
ASTM D4883
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength at Break 27.0 MPa
3920 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 23.0 MPa
3340 psi
2 in/min.; ASTM D638
Elongation at Break >= 600 %
>= 600 %
2 in/min.; ASTM D638
Descriptive Properties Value Comments
Process Pipe Extrusion