Izod Impact, Notched 0.908 J/cm

@Temperature 22.8 °C
1.70 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
Izod Impact, Notched 0.908 J/cm

@Temperature -30.0 °C
1.70 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Polymer Resources PPX-G15 Modified-PPO, 15% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Izod Impact, Notched 0.908 J/cm

@Temperature -20.0 °C
1.70 ft-lb/in

@Temperature -4.00 °F
1/8'' notched bar; ASTM D256
Ineos 3560 Polypropylene Impact Copolymer
This is a special high melt flow, nucleated, high impact copolymer polypropylene for injection molding applications. It offers excellent impact resistance and a high flexural modulus.ApplicationsAu..
Izod Impact, Notched 0.908 J/cm

@Temperature -20.0 °C
1.70 ft-lb/in

@Temperature -4.00 °F
1/8'' notched bar; ASTM D256
Ineos T20N-00 Polypropylene Impact Copolymer
This is a special high melt flow, nucleated, high impact copolymer polypropylene for injection molding applications. It offers excellent impact resistance and a high flexural modulus.ApplicationsCo..
Izod Impact, Notched 0.908 J/cm

@Temperature -17.8 °C
1.70 ft-lb/in

@Temperature 0.000 °F
1/8" x 1/2" bar; ASTM-D256 (Method A)
Ineos ABS Lustran® Guardian™ 620 ABS, Extrusion Grade
Lustran® Guardian™ ABS 620 is a high modulus, HFC 134a and HCFC 22 resistant extrusion grade resin designed for refrigerator door and food liners. Lustran® ABS 620 offers good melt streng..
Izod Impact, Notched 0.908 J/cm

@Thickness 6.35 mm
1.70 ft-lb/in

@Thickness 0.250 in
ASTM D256
PlastxWorld CEVIAN®-V T180 ABS
High Modulus ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Izod Impact, Notched 0.908 J/cm

@Temperature -18.0 °C
1.70 ft-lb/in

@Temperature -0.400 °F
ASTM D256
Formosa Plastics Formolene® 6610A Impact Copolymer Polypropylene
Impact Copolymer for Compounding and Injection Molded Applications Formolene® 6610A is a high impact copolymer of polypropylene designed for such injection applications as automotive compounding, l..
Izod Impact, Notched 0.908 J/cm

@Temperature 22.8 °C
1.70 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Clariant ABS4500 ABS, High Impact
Data provided by Clariant Masterbatches
Izod Impact, Notched 0.908 J/cm

@Temperature 22.8 °C
1.70 ft-lb/in

@Temperature 73.0 °F
ASTM D256A
ExxonMobil AP3AW Polypropylene Impact Copolymer
Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe..
Copyright © lookpolymers.com All Rights Reserved