Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT550 Heat Treatment)

Category Metal , Ferrous Metal , Martensitic , Stainless Steel , T S40000 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name SOLEIL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT550 Heat Treatment).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The grade has a martensitic microstructure. The final mechanical properties may be optimized by selecting an appropriate heat treatment. In the annealed conditions the alloy presents ductility and may be formed. Chromium additions (~13%) improve the corrosion resistance, particularly in wet conditions when compared to C-Mn steels. Slightly acidified and abrasion conditions are considered. The main applications concern mechanical industry, oil and gas industry, sugar industry and constructional components.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 160
160
Typical
Tensile Strength, Ultimate 550 - 750 MPa
79800 - 109000 psi
Minimum Guaranteed
Tensile Strength, Yield >= 400 MPa
>= 58000 psi
Minimum Guaranteed
Elongation at Break >= 15 %
>= 15 %
Modulus of Elasticity 212 GPa
30700 ksi
Charpy Impact 85.0 J
62.7 ft-lb
Typical Toughness (long)
Thermal Properties Metric English Comments
CTE, linear 10.5 µm/m-°C

@Temperature 20.0 - 100 °C
5.83 µin/in-°F

@Temperature 68.0 - 212 °F
11.0 µm/m-°C

@Temperature 20.0 - 200 °C
6.11 µin/in-°F

@Temperature 68.0 - 392 °F
11.5 µm/m-°C

@Temperature 20.0 - 300 °C
6.39 µin/in-°F

@Temperature 68.0 - 572 °F
12.0 µm/m-°C

@Temperature 20.0 - 500 °C
6.67 µin/in-°F

@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 25.0 W/m-K

@Temperature 20.0 °C
174 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Carbon, C 0.12 %
0.12 %
Chromium, Cr 12.5 %
12.5 %
Iron, Fe 86.48 %
86.48 %
As remainder
Manganese, Mn 0.50 %
0.50 %
Silicon, Si 0.40 %
0.40 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000600 ohm-cm

@Temperature 20.0 °C
0.0000600 ohm-cm

@Temperature 68.0 °F