Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 120 °C | 248 °F | |
Indium Corp. Indalloy 64 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 120 °C | 248 °F | |
Indium Corp. Indalloy 89 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 120 °C | 248 °F | |
Indium Corp. Indalloy 98 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |