Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 152 °C | 306 °F | |
Indium Corp. Indalloy 230 Indium-Tin-Lead Solder Alloy Also known as 532Information Provided by Indium Corporation |
|||
Liquidus | 152 °C | 306 °F | |
Indium Corp. Indalloy 532 Tin Solder Alloy Also known as 230Information Provided by Indium Corporation |
|||
Liquidus | 152 °C | 306 °F | |
Indium Corp. Indalloy 89 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Liquidus | 152 °C | 306 °F | |
Indium Corp. Indalloy 90 Indium Solder Alloy Information Provided by Indium Corporation |