Polymer Property : Solidus = 118 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 118 °C
244 °F
Indium Corp. Indalloy 71 Indium-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 118 °C
244 °F
Indium Corp. Indalloy 87 Indium-Tin Solder Alloy
Information Provided by Indium Corporation
Solidus 118 °C
244 °F
Indium Corp. Indalloy 1 Indium-Tin Solder Alloy
Fair wettability on glass, quartz, and many ceramics. Good low temperature malleability. Compensates for some CTE mismatch. Low vapor pressureInformation Provided by Indium Corporation
Solidus 118 °C
244 °F
Indium Corp. Indalloy® 1E In-Sn Solder Alloy
Lowest melting point practical solder. Indium-tin eutectic with sharp melting point. Has good wettability on glass, quartz and many ceramics. Has good low temperature malleability and therefore com..
Solidus 118 °C
244 °F
Williams Advanced Alloys WS118 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Solidus 118 °C
244 °F
Williams Advanced Alloys WS145 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Solidus 118 °C
244 °F
AIM 52In/48Sn Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.