Thermal Properties Metric English Comments
Thermal Conductivity 34.0 W/m-K

@Temperature 20.0 °C
236 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC)
Description: CLC 1.2311 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, carbon and manganese additions are optimized to have a fully martens..
Thermal Conductivity 34.0 W/m-K

@Temperature 20.0 °C
236 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability
Description: CLC 1.2312 is a chromium-manganese-molybdenum grade designed for plastic mold industry. This grade is normally delivered in a prehardened condition at a hardness level of 300HB/32HRC. T..
Thermal Conductivity 34.0 W/m-K

@Temperature 1100 °C
236 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes 214® alloy sheet
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 34.0 W/m-K

@Temperature 1100 °C
236 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes 214® alloy, sheet, 100 hours exposure at 760°C (1400°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 34.0 W/m-K

@Temperature 1100 °C
236 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes 214® alloy, sheet, 100 hours exposure at 870°C (1600°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 34.0 W/m-K

@Temperature 1100 °C
236 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes 214® alloy, sheet, 100 hours exposure at 980°C (1800°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 34.0 W/m-K

@Temperature 1100 °C
236 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes 214® alloy, sheet, 1000 hours exposure at 760°C (1400°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 34.0 W/m-K

@Temperature 1100 °C
236 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes 214® alloy, sheet, 1000 hours exposure at 870°C (1600°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 34.0 W/m-K

@Temperature 1100 °C
236 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes 214® alloy, sheet, 1000 hours exposure at 980°C (1800°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 34.0 W/m-K

@Temperature 1100 °C
236 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes 214® alloy, sheet, 32 hours exposure at 760°C (1400°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 34.0 W/m-K

@Temperature 1100 °C
236 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes 214® alloy, sheet, 32 hours exposure at 870°C (1600°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 34.0 W/m-K

@Temperature 1100 °C
236 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Haynes 214® alloy, sheet, 32 hours exposure at 980°C (1800°F)
Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh ..
Thermal Conductivity 34.0 W/m-K

@Temperature 85.0 °C
236 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy 1 Indium-Tin Solder Alloy
Fair wettability on glass, quartz, and many ceramics. Good low temperature malleability. Compensates for some CTE mismatch. Low vapor pressureInformation Provided by Indium Corporation
Thermal Conductivity 34.0 W/m-K

@Temperature 85.0 °C
236 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 1E In-Sn Solder Alloy
Lowest melting point practical solder. Indium-tin eutectic with sharp melting point. Has good wettability on glass, quartz and many ceramics. Has good low temperature malleability and therefore com..
Thermal Conductivity 34.0 W/m-K
236 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS118 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys