Polymer Property : Electrical Resistivity = 0.0000150 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000150 ohm-cm
0.0000150 ohm-cm
Nihon Superior SN100CL Lead-Free Solder Alloy
Used for hot air solder leveling (HASL). Features include: Excellent fluidity; Bridge-free coating of the fine pitch circuitry; Bright smooth and uniform coating; Low copper erosion; Formation of st..
Electrical Resistivity 0.0000150 ohm-cm
0.0000150 ohm-cm
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy
Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation.
Electrical Resistivity 0.0000150 ohm-cm
0.0000150 ohm-cm
Indium Corp. Indalloy 109 Tin-Lead Solder Alloy
Good electrical grade solderInformation Provided by Indium Corporation
Electrical Resistivity 0.0000150 ohm-cm
0.0000150 ohm-cm
Indium Corp. Indalloy® 1E In-Sn Solder Alloy
Lowest melting point practical solder. Indium-tin eutectic with sharp melting point. Has good wettability on glass, quartz and many ceramics. Has good low temperature malleability and therefore com..
Electrical Resistivity 0.0000150 ohm-cm
0.0000150 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
California Fine Wire Nickel Alloy 90 Copper Nickel Resistance Wire
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Electrical Resistivity 0.0000150 ohm-cm
0.0000150 ohm-cm
ATI Wah Chang Niobium
Niobium is a soft, ductile metal which can be cold worked over 90 percent before annealing becomes necessary. In appearance, the metal is somewhat similar to stainless steel. The density of 8.57 gm/..