Material Notes:
EPK Kaolin is a unique, high quality water washed ceramic kaolin which offers very white fired color, unusually good forming characteristics and high green strength. In glaze, EPK offers excellent suspension capabilities and uncommon cleanliness.Information provided by Imerys
Physical Properties Metric English Comments
Bulk Density 0.513 g/cc
0.0185 lb/in³
loose
0.737 g/cc
0.0266 lb/in³
packed
Particle Size 1.0 µm
1.0 µm
average
Particle Mesh Size 325 Mesh
325 Mesh
1.6% retained, pellet (prill)
325 Mesh
325 Mesh
1.2% retained, airfloated
pH 6.0
6.0
Specific Surface Area 25.6 m²/g
25.6 m²/g
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00207 GPa
0.300 ksi
Component Elements Properties Metric English Comments
Al2O3 37.4 %
37.4 %
CaO 0.18 %
0.18 %
Fe2O3 0.79 %
0.79 %
K2O 0.33 %
0.33 %
Loss on Ignition(%) 13.9 %
13.9 %
MgO 0.10 %
0.10 %
P2O5 0.24 %
0.24 %
SiO2 45.7 %
45.7 %
TiO2 0.37 %
0.37 %
Processing Properties Metric English Comments
Moisture Content 1.0 %
1.0 %
Plus 325 Mesh (Airfloated)
3.0 %
3.0 %
Plus 325 Mesh (Pellet/Prill)
Descriptive Properties Value Comments
M.B.I. (meq/100g) 3.7