Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00207 GPa | 0.300 ksi | De-aired, Extruded, 50% Kaolin/50% Flint |
Imerys Allenâ„¢ G Kaolin Allen G is an intermediate-grained kaolin used as a suspension aid in ceramic glazes.Information provided by Imerys |
|||
Modulus of Rupture | 0.00207 GPa | 0.300 ksi | |
Imerys EPK Kaolin EPK Kaolin is a unique, high quality water washed ceramic kaolin which offers very white fired color, unusually good forming characteristics and high green strength. In glaze, EPK offers excellent s.. |
|||
Modulus of Rupture | 0.00207 GPa | 0.300 ksi | |
Imerys Hamiltonâ„¢ Kaolin Hamilton is a fine-grained kaolin with low alkali content and high PCE. These properties make for ideal air-set refractory mortars. Halloysite content provides excellent suspension and trowel abilit.. |
|||
Modulus of Rupture | 0.00207 GPa | 0.300 ksi | dry |
Imerys Kaolin Slurryâ„¢ Kaolin Slurry is a carefully controlled Kaolin-water suspension formulated for use in cermic castings.Information provided by Imerys |
|||
Modulus of Rupture | 0.00207 GPa | 0.300 ksi | parallel to thickness |
Zircar Refractory Composites RS-99-45 Refractory Sheet ZRCI Refractory Sheet Type RS-99-45 is comprised of 99% alumina. This "All-Alumina" material is strong, uniform, rigid, refractory structure composed of alpha alumina fibers and high purity inorgani.. |
|||
Modulus of Rupture | 0.00207 GPa | 0.300 ksi | Green (typ.) |
Unifrax Fiberfrax® Duraboard® HD Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |