Polymer Property : Bulk Density = 0.513 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.513 g/cc
0.0185 lb/in³
loose
Imerys EPK Kaolin
EPK Kaolin is a unique, high quality water washed ceramic kaolin which offers very white fired color, unusually good forming characteristics and high green strength. In glaze, EPK offers excellent s..
Bulk Density 0.513 g/cc
0.0185 lb/in³
DayGlo Gem-Tone GC-13P Ruby Red
Gem-Tone® GC-13P Ruby Red is a rich, strong blue shade red colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use..
Bulk Density 0.513 g/cc
0.0185 lb/in³
DayGlo Gem-Tone GC-18F Emerald Green
Gem-Tone® GC-18F Emerald Green is a rich, strong green colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use of ..