Physical Properties Metric English Comments
Bulk Density 0.737 g/cc
0.0266 lb/in³
packed
Imerys EPK Kaolin
EPK Kaolin is a unique, high quality water washed ceramic kaolin which offers very white fired color, unusually good forming characteristics and high green strength. In glaze, EPK offers excellent s..
Bulk Density 0.737 - 0.785 g/cc
0.0266 - 0.0284 lb/in³
Aggregate, dried, 14 x 40 mesh
St. Cloud Natural Zeolite (Clinoptilolite)
Natural zeolites are microporous volcanic minerals with sieving and cation exchange properties for use in agriculture, environmental and industrial applications. Features such as a vary large inter..