Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 323.4 W/m-K | 2244 BTU-in/hr-ft²-°F | |
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi.. |
|||
Thermal Conductivity | 323.4 W/m-K | 2244 BTU-in/hr-ft²-°F | |
Cadi 1815 Copper Alloy Zirconium addition to chromium copper improves creep resistance at high operating temperatures and reportedly reduces sticking of electrodes to the work during spot welding of galvanized materials. .. |
|||
Thermal Conductivity | 323.4 W/m-K | 2244 BTU-in/hr-ft²-°F | |
Cadi 182 Copper Alloy Chromium copper is the primary copper alloy used for resistance spot and seam welding. This alloy achieves good hardness and electrical conductivity through a combination of heat treatment and cold .. |