Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000200 ohm-cm | 0.00000200 ohm-cm | |
OMG Americas GlidCop® AL-25 Dispersion Strengthened Copper GlidCop® AL-25 is copper that is dispersion strengthened with 0.5 wt% ultrafine particles of aluminum oxide. It is produced using an internal oxidation powder metallurgy process whereby aluminum o.. |
|||
Electrical Resistivity | 0.00000200 ohm-cm | 0.00000200 ohm-cm | Plate and Rounds |
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi.. |
|||
Electrical Resistivity | 0.00000200 - 0.00000400 ohm-cm | 0.00000200 - 0.00000400 ohm-cm | In-Plane; ASTM-C611 |
GrafTech GRAFCELL® GDB Graphite Gas Diffusion Barrier GRAFCELL® Gas Diffusion Barrier (GDB) material is a thin, perforated structure made from a continuous matrix of expanded natural graphite with excellent electrical conductivity, thermal conductiv.. |
|||
Electrical Resistivity | 0.00000200 ohm-cm | 0.00000200 ohm-cm | |
Lucas-Milhaupt Silvaloy® B72 Brazing Alloy Silvaloy B72 is the eutectic composition of the silver-copper system. It is suitable for use in controlled atmosphere brazing without the use of a paste flux. When molten, it is very fluid and may f.. |
|||
Electrical Resistivity | 0.00000200 ohm-cm | 0.00000200 ohm-cm | |
Goodfellow Tungsten Carbide/Cobalt Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard cerami.. |
|||
Electrical Resistivity | 0.00000200 ohm-cm | 0.00000200 ohm-cm | 84 % IACS |
CMW® ELKONIUM 22 silver, copper alloy Alloying copper into silver increases the hardness of the material, and its resistance to mechanical wear and deformation. The electrical and thermal conductivity remain relatively high, thus, the a.. |