Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 496 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 496 MPa

@Temperature 21.1 °C
72000 psi

@Temperature 70.0 °F
0° Direction, Dry; ASTM D638
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Tensile Strength, Yield 496 - 565 MPa

@Strain 0.200 %
72000 - 82000 psi

@Strain 0.200 %
Plate and Rounds
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper
C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi..
Tensile Strength, Yield 496 MPa

@Strain 0.200 %
71900 psi

@Strain 0.200 %
Haynes Ultimet® alloy, 1.6 mm sheet
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Tensile Strength, Yield 496 MPa

@Strain 0.200 %
71900 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 496 - 558 MPa
72000 - 81000 psi
0.2% offset
Eagle Brass 735 Nickel Silver 18%, Extra Hard
735 is used for coinage, name plates, zippers, flatware, and fashion jewelry.Information provided by Eagle Brass Company
Tensile Strength, Yield 496 MPa

@Strain 0.200 %,
Temperature 760 °C
71900 psi

@Strain 0.200 %,
Temperature 1400 °F
Carpenter Thermo-Span® Fe-Co-Ni Superalloy
Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h..
Tensile Strength, Yield 496 MPa

@Strain 0.200 %
71900 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, SMAW weld, 904L base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..