Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman PE2053 Injection Molding Polyethylene  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman PE2053 Injection Molding Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer, Drug Master File listed product, and FDA compliant.Features: High flow characteristics, good gloss, and processability.Applications: Injection molding: large moldings including housewares and toys.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170Information provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 24 g/10 min
24 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
ASTM D2240
Tensile Strength, Ultimate 10.0 MPa
1450 psi
ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Modulus of Elasticity 0.248 GPa
36.0 ksi
Secant; ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 88.0 °C
190 °F
ASTM D1525
Users viewing this material also viewed the following: