Polymer Property : Melt Flow = 24 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133B
Mytex Polymers AS171L-02US Polypropylene, 13% Talc Filled
AS171L-02US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability.This product is available ..
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
SABIC PP 5707N Polypropylene Homopolymer STIFFPACT for Injection Molding
Product Description: PP 5707N is a reactor PP homopolymer grade with antistatic and nucleated agents. It is suitable for producing injection molded applications and gives consistent processability..
Melt Flow 24 g/10 min

@Load 5.00 kg,
Temperature 260 °C
24 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
Melt Flow 24 - 26 g/10 min
24 - 26 g/10 min
ASTM D1238
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
PolyMirae Moplen HP640R Injection Molding Grade Polypropylene
Moplen HP640R is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640R is a homopolymer particularly suitable for injection molding..
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
PolyMirae Moplen RP344R Injection Molding Grade Polypropylene
Moplen RP344R is a nucleated polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP344R is a random copolymer particularly suitable for..
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133 B
Mytex Polymers AS319L-01US Thermoplastic Polyolefin, 19% Talc Filled
AS319L-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural or ..
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Yparex 8125 Polyolefin Adhesive Resin
The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer..
Melt Flow 24 g/10 min
24 g/10 min
melt index; ASTM D1238
Asahi Kasei Tenac® 5012 Acetal Homopolymer  (discontinued **)
Standard-flow grade, with reduced stiffness and increased elongation through addition of special polymers.Applications: Clips, fasteners, press-fit parts.This product is not a part of the standard p..
Melt Flow 24 g/10 min
24 g/10 min
ISO 1133
LATI LATAN 23 Polyoxymethylene Copolymer (POM)  (discontinued **)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
Melt Flow 24 g/10 min
24 g/10 min
Condition I; ASTM D1238
Plaskolite Optix® PL-200 Acrylic Resin  (discontinued **)
Injection molding grade pellets.Data provided by the manufacturer, Plaskolite, Inc.
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical LUTENE MB9205 LDPE Injection Molding Grade
Description: The physical and structural characteristics of LUTENE MB9205 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Lids of all sizes, hous..
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
LG Chemical LUTENE MB9500 LDPE Injection Molding Grade
Description: The physical and structural characteristics of LUTENE MB9500 give it excellent flow properties and good productivity, clarity and surface gloss.Main Application: Powder coating, artific..
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
IRPC Polimaxx Polene 3370RM Polypropylene Random Copolymer
CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD ADHESIVE, GOOD CLARITY, LOW NECK IN/ODOR HIGH SPEED APPLICATIONS: EXTRUSION COATING FOR COATED OPP FILM
Melt Flow 24 g/10 min

@Load 5.00 kg,
Temperature 200 °C
24 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Kraton® D1113 P (SIS) Linear Block Copolymer
Description: Kraton D1113 P is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 16%. It is supplied from North America in the physical form identified: Kra..
Melt Flow 24 g/10 min

@Load 5.00 kg,
Temperature 300 °C
24 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Melt Flow 24 g/10 min

@Load 6.60 kg,
Temperature 337 °C
24 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant.
Melt Flow 24 g/10 min

@Load 6.60 kg,
Temperature 337 °C
24 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE (Asia Pacific)
High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant.
Melt Flow 24 g/10 min

@Load 6.60 kg,
Temperature 337 °C
24 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM AUT195 PEI+PCE
High flow Polyetherimide blend for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 195C (SABIC test method).
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
SK Chemicals SKYPEL M572CR Special Grade Copper Resistance
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Melt Flow 24 g/10 min

@Load 5.00 kg,
Temperature 250 °C
24 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
Melt Flow 24 g/10 min
24 g/10 min
ISO 1133
Domo 1101S Polypropylene Homopolymer
Information provided by Domo.
Melt Flow 24 - 36 g/10 min
24 - 36 g/10 min
Asahi Glass Fluon® P-62XP PFA Perfluoropolymer
Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character..
Melt Flow 24 g/10 min

@Load 1.20 kg,
Temperature 300 °C
24 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Covestro Makrolon® Rx1851 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..
Melt Flow 24 g/10 min

@Load 1.20 kg,
Temperature 275 °C
24 g/10 min

@Load 2.65 lb,
Temperature 527 °F
DAM; cm³/10min; ISO 1133
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Radici Heraform® R 3000 Acetal Copolymer
Very easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Radici group.
Melt Flow 24 g/10 min

@Load 10.0 kg,
Temperature 220 °C
24 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Infino® NH-3208GL PC, Glass Filled FR
Information provided by Samsung Cheil Industries.
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
IRPC Polimaxx Polene 3375RM Polypropylene Random Copolymer
CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD ADHESIVE, HIGH SPEED APPLICATIONS: EXTRUSION COATING FOR COATED WOVEN BAGS AND TARPAULINS
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
from MVR; ISO 1033
Sax Polymers SAXALEN PPC344G25 Polypropylene Copolymer, 25% Glass Filled
SAXALEN PPC344G25 is a 25% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 190 °C
24 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
M. Holland Company LL500 LLDPE  (discontinued **)
Features: Medium Flow, Good ProcessabilityUses: Blending, Color ConcentratesProcessing Method: Injection MoldingInformation provided by M. Holland.