Material Notes:
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
ASTM D2240
Tensile Strength at Break 24.1 MPa
3500 psi
ASTM D412
Elongation at Break 850 %
850 %
ASTM D412
100% Modulus 0.00172 GPa
0.250 ksi
ASTM D412
300% Modulus 0.00276 GPa
0.400 ksi
ASTM D412
Tear Strength 39.4 kN/m
225 pli
ASTM D624
Peel Strength 14.0 kN/m

@Temperature 85.0 °C
80.0 pli

@Temperature 185 °F
resistance to glass; ASTM D3167
18.4 kN/m

@Temperature 90.5 °C
105 pli

@Temperature 195 °F
resistance to glass; ASTM D3167
23.7 kN/m

@Temperature 99.0 °C
135 pli

@Temperature 210 °F
resistance to glass; ASTM D3167
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -49.0 °C
-56.2 °F
Processing Properties Metric English Comments
Melt Temperature 60.0 - 110 °C
140 - 230 °F