Polymer Property : Peel Strength = 14.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 14.0 kN/m

@Temperature 85.0 °C
80.0 pli

@Temperature 185 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 429 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Peel Strength 14.0 kN/m

@Temperature 85.0 °C
80.0 pli

@Temperature 185 °F
resistance to glass; ASTM D3167
Huntsman KRYSTALFLEX® PE 499 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers