Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00172 GPa | 0.249 ksi | ASTM D412 |
Network Polymers Softflex® 0921 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Non-Black Sulfur Cure Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.249 ksi | |
Shin-Etsu Silicones LIMSâ„¢ KEG2000-50A/B Elastomer KEG2000-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | >= 0.00172 GPa | >= 0.250 ksi | Compound Property |
Arlon 10502N060 0.060" (1.52 mm) Cured/Post-Cured Unsupported Silicone Rubber Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used t.. |
|||
100% Modulus | >= 0.00172 GPa | >= 0.250 ksi | Compound Property |
Arlon 10502R030 0.040" (1.02 mm) Cured/Post-Cured Unsupported Silicone Rubber Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used t.. |
|||
100% Modulus | >= 0.00172 GPa | >= 0.250 ksi | |
Arlon 10502R125 Cured/Post-cured, Unsupported Silicone Rubber Product Color: RedInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silic.. |
|||
100% Modulus | >= 0.00172 GPa | >= 0.250 ksi | |
Arlon 30400N125 0.125" (3.17 mm) Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a Kodacel Carrier Appearance: Translucent silicone rubber on polymer linerThis data represents typical values for the production ma.. |
|||
100% Modulus | >= 0.00172 GPa | >= 0.250 ksi | Tension, Silicone Property |
Arlon 41400R030 0.030" Uncured, Unsupported Silicone Rubber on a Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
100% Modulus | 0.00172 GPa | 0.249 ksi | Average |
Arlon Thermavac® 0.030" (0.762 mm) Uncured Silicone Vacuum Bagging (30400N030) Uncured, unsupported silicone rubber with a thickness of 0.030 in ± 0.003 (0.76 mm ± 0.038) on a Kodacel carrier (0.005 in., 0.13 mm nominal thickness); 0.003 in. (0.8 mm) polyethylene interleave... |
|||
100% Modulus | 0.00172 GPa | 0.249 ksi | Average |
Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502N060) Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15 ); 0.003 in. (0.8 mm) polyethylene interleave. Color: Translucent. Weight: 2339 g/m² ± 234 (69.0.. |
|||
100% Modulus | 0.00172 GPa | 0.249 ksi | Average |
Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502R060) Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15); 0.003 in. (0.8 mm) polyethylene interleave. The shelf life is defined as the duration of time for.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | ASTM D638 |
Colorite Polymers 4875 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Atomite Whiting Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00172 GPa | 0.250 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR N330 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |